Ok,. today was another attempt to encase in clear without cooking the clear and turning it into a carbon filled grey scum layer over the beads.
The first bead was a warmup bead,lol. It is an implosion bead. This bead went through a process of almost turning itself inside-out to get the look of this flower. Love doing these.
The second bead is actually my second attempt at a plunged dot floral. Both of these beads are 16mm and the clear stayed nice and clear. No carbon scum here yaaay!

The orange petal floral was my first attempt at a plunged dot floral. I have not read any instructions how to do these yet and did these the way I thought they were made. This bead is a whopper at 1″ and covered in a carbon scum from letting the clear heat up too much. Oh well,lol. The white petalled bead is my third attempt at a plunged dot floral and is supposed to be slightly pinkish since the white petals were covered in transparent amethyst. Unfortunately this bead also suffered a roasting,lol and is also covered in a carbon scum layer. The petals looks rather grey in real like *snif*.
Soooooh it seems that I can avoid cooking the clear when doing small beads,.. but large beads I just cook ‘em. It seems my options are,.. melt mid-flame and get carbon scum,.. melt high in flame and die of old age while waiting for the glass to form it’s nice round shape. I think I will try again after reading some instructions first, and try and figure out the clear trick. Clear and I,… we just don’t get along :} .